Effects of mechanical and thermal load cycling on micro tensile bondstrength of clearfil SE bond to superficial dentin
چکیده:   (1883 مشاهده)

 Background: Certain studies have been conducted on the effects of mechanical and thermal loadcycling on the microtensile bond strength (microTBS) of composites to dentin, but the resultswere different. The authors therefore decided to evaluate these effects on the bonding of ClearfilSE bond to superficial dentin.

 Materials and Methods: Flat dentinal surface of 42 molar teeth were bonded to Filtek‑Z250 resincomposite by Clearfil SE bond. The teeth were randomly divided into 7 groups and exposed to differentmechanical and thermal load cycling. Thermocycling was at 5‑55‹C and mechanical load cycling wascreated with a force of 125 N and 0.5 Hz. Then, the teeth were sectioned and shaped to hour glass formand subjected to microTBS testing at a speed of 0.5 mm/min. The results were statistically analyzed bycomputer with three‑way analysis of variance and T‑test at P < 0.05 significant. To evaluate the locationand mode of failure, the specimens were observed under the stereomicroscope. Then, one of thespecimens in each group was evaluated under Scanning Electron Microscopy (SEM) for mode of failure.

 Results: All of the study groups had a significantly lower microTBS as compared to the control group (P < 0.001). There was no statistically significant difference between mechanical cycling with50K (kilo = 1000) cycles, and 50K mechanical cycles plus 1K thermal cycles. Most of the fracturesin the control group were of adhesive type and this type of fracture increased after exposure tomechanical and thermal load cycling.

 Conclusion: Thermal and mechanical load cycling had significant negative effects on microTBS andthe significant effects of mechanical load cycling started to be significant at 100K cycles.


 Source: Dental Research Journal

 Full Text

     
نوع مطالعه: پژوهشي | موضوع مقاله: ترمیمی
دریافت: 1392/4/16 | پذیرش: 1394/9/25 | انتشار: 1394/9/25
ارسال نظر درباره این مقاله
نام کاربری یا پست الکترونیک شما:

CAPTCHA


XML   English Abstract   Print


Download citation:
BibTeX | RIS | EndNote | Medlars | ProCite | Reference Manager | RefWorks
Send citation to:

Daneshkazemi A, Davari A R, Ataei E, Dastjerdi F, Hajighasemi E. Effects of mechanical and thermal load cycling on micro tensile bondstrength of clearfil SE bond to superficial dentin. 3 2012;
URL: http://idai.ir/article-1-1216-fa.html

Effects of mechanical and thermal load cycling on micro tensile bondstrength of clearfil SE bond to superficial dentin. 1. 1390;

URL: http://idai.ir/article-1-1216-fa.html



بازنشر اطلاعات
Creative Commons License این مقاله تحت شرایط Creative Commons Attribution-NonCommercial 4.0 International License قابل بازنشر است.
جلد 0 - ترمیمی برگشت به فهرست نسخه ها
جامعه اسلامی دندانپزشکان Islamic Dental Association of IRAN

کلیه حقوق سایت متعلق به جامعه اسلامی دندانپزشکان ایران است. تماس با ما

Persian site map - English site map - Created in 0.04 seconds with 37 queries by YEKTAWEB 4710