Initial fracture resistance and curing temperature rise of ten contemporary resin-based composites with increasing radiant exposure
چکیده:   (1288 مشاهده)

 Objectives

  The principal objective of this study was to determine whether the bulk fracture resistance of ten light activated composites varied over a clinically realistic range of radiant exposures between 5 and 40J/cm2.

  Methods

  Ten operators were tested for clinically simulated radiant exposure delivery from a Bluephase® (Ivoclar Vivadent, Schaan, Liechtenstein) LED light to an occlusal cavity floor in tooth 27 in a mannequin head using a MARC®-Patient Simulator (Bluelight Analytics Inc., Halifax, NS) device. Notch disc test samples were prepared to determine the torque resistance to fracture (T) of the composites. Samples were irradiated with the same monowave Bluephase® light for 10s, 20s or 40s at distances of 0mm or 7mm. After 24h, storage samples were fractured in a universal testing machine and torque to failure was derived.

  Results

  Radiant exposure delivered in the clinical simulation ranged from 14.3% to 69.4% of maximum mean radiant exposure deliverable at 0mm in a MARC®-Resin Calibrator (Bluelight Analytics Inc., Halifax, NS) test device. Mean torque to failure increased significantly (P<0.05) with radiant exposure for 8 out of 10 products. The micro-fine hybrid composite Gradia Direct anterior (GC) had the lowest mean (S.D.) T between 10.3 (1.8)N/mm and 13.7 (2.2)N/mm over the tested radiant exposure range. Three heavily filled materials Majesty Posterior, Clearfil APX and Clearfil Photo-Posterior (Kuraray) had mean T values in excess of 25N/mm following 40J/cm2 radiant exposure. Mean T for Z100 (3MESPE) and Esthet-X (Dentsply) increased by 10% and 91% respectively over the tested range of radiant exposures.

 Conclusions

 Individual products require different levels of radiant exposure to optimize their fracture resistance. Light activated composites vary in the rate at which they attain optimal fracture resistance.

 Clinical significance

 Unless the clinician accurately controls all the variables associated with energy delivery, there is no way of predicting that acceptable fracture resistance will be achieved intra-orally.


 Source: Journal of Dentistry

 Full Text

واژه‌های کلیدی: Fracture، Composite، Exotherm، Radiant exposure، Curing
     
نوع مطالعه: پژوهشي | موضوع مقاله: ترمیمی
دریافت: 1392/7/15 | پذیرش: 1394/9/25 | انتشار: 1394/9/25
ارسال نظر درباره این مقاله
نام کاربری یا پست الکترونیک شما:

CAPTCHA


XML     Print


Download citation:
BibTeX | RIS | EndNote | Medlars | ProCite | Reference Manager | RefWorks
Send citation to:


Initial fracture resistance and curing temperature rise of ten contemporary resin-based composites with increasing radiant exposure. 1. 1390;

URL: http://idai.ir/article-1-2177-fa.html



بازنشر اطلاعات
Creative Commons License این مقاله تحت شرایط Creative Commons Attribution-NonCommercial 4.0 International License قابل بازنشر است.
جلد 0 - ترمیمی برگشت به فهرست نسخه ها
جامعه اسلامی دندانپزشکان Islamic Dental Association of IRAN

کلیه حقوق سایت متعلق به جامعه اسلامی دندانپزشکان ایران است. تماس با ما

Persian site map - English site map - Created in 0.05 seconds with 37 queries by YEKTAWEB 4710